Dielines › Dielines by standard code › ECMA X29
ECMA X29 — Perforated tear-off lid around the body
ECMA X29 is a single perforation line around the carton body that lets the top be torn off as a lid. Drint draws a free ECMA X29 dieline at any size: type the length, width and height and design on it, or download it as PDF or SVG with Pro.

- Code
- ECMA X29
- Standard
- ECMA — folding carton
- Group
- ECMA X · Locks and auxiliary features
- Drawn at
- 80 × 50 × 140 mm
- Flat sheet
- 274 × 270 mm
- Also called
- Tear-off lid along the length perforation
- Drawing
- Close to the code’s drawing, not exact
In Claude or ChatGPT, add the Drint connector (drint.io/mcp) and ask: “ECMA X29 dieline, 300 × 200 × 100 mm, PDF”.
How it folds
X29 uses one perforated line rather than a two-cut strip: it runs round the body 28 mm below the top, with a pull notch at the edge of the back panel. Drint shows it on an 80 × 50 × 140 mm tuck-end carton. The geometry is Drint's own in the style of the code; set the perforation cut-and-tie with the box maker.
What it is used for
Simple tamper evidence and easy opening on cartons for snacks, tea, tissues, pharmaceuticals and consumer goods. It is cheaper than a zipper strip and leaves a cleaner edge on the base.
Blank size by box size
The flat sheet a ECMA X29 needs at each box size, measured on Drint’s own dieline with the board’s thickness allowed for. Add your press’s trim and gripper margin. Each size opens the die in the studio.
| Box, L × W × H | Flat sheet | Sheet area |
|---|---|---|
| 40 × 25 × 70 mm | 144 × 150 mm | 0.02 m² |
| 55 × 35 × 100 mm | 194 × 200 mm | 0.04 m² |
| 80 × 50 × 140 mm | 274 × 270 mm | 0.07 m² |
| 105 × 65 × 180 mm | 354 × 340 mm | 0.12 m² |
| 130 × 80 × 225 mm | 434 × 415 mm | 0.18 m² |
| 160 × 100 × 280 mm | 534 × 510 mm | 0.27 m² |
Measured by Drint’s die engine
These numbers are measured on the ECMA X29 die at 80 × 50 × 140 mm, drawn by the same engine as the studio — not copied from a catalogue.
| Cutting rule | 1.30 m |
|---|---|
| Creasing rule | 1.08 m |
| Perforation | 0.27 m |
| Total rule per copy | 2.65 m |
| Blank area (board in the box) | 0.055 m² |
| Share of the bounding box used | 73.9% |
| Board per 1,000 blanks (bounding box) | 74 m² |
| Best press sheet | 60 × 84 cm: 6 up, 65.1% of the sheet used |
Parts of this die: Glue flap · Dust flap · Tuck flap · Closure panel · Front panel · Side panel · Back panel
Board
Folding boxboard 250–350 gsm. The perforation must be strong enough for transit but weak enough to tear by hand; laminated board needs a test.
Printing and die notes
Mark the start at the notch and show a dotted tear line in the artwork if helpful. Avoid placing important copy right on the perforation.
Common mistakes
- Perforation ties too weak, so the box opens in transit.
- Ties too strong, so the board tears away from the line.
- Barcode printed across the perforation.
Questions
What is ECMA X29?
ECMA X29 is a single perforation line around the carton body that lets the top be torn off as a lid.
How does X29 differ from X13?
X29 is a single perforation line; X13 is a 5 mm strip removed between two lines.
Where does tearing start?
At the pull notch on the back panel edge.
What size sheet does a 80 × 50 × 140 mm ECMA X29 need?
A ECMA X29 of 80 × 50 × 140 mm unfolds to a flat sheet of 274 × 270 mm (0.07 m²) on Drint’s dieline, before trim and gripper margins. The table on this page gives the sheet for other sizes; in the studio, type any length, width and height and the sheet is measured again.
How do I get a ECMA X29 dieline at my size?
Open it in Drint and type your length, width and height — inside, on the crease or outside. The die is redrawn at that size with the board’s thickness allowed for, and you design straight on it. In Claude or ChatGPT with the Drint connector, ask for “ECMA X29 dieline” and your size.
What board is ECMA X29 made from?
Folding boxboard 250–350 gsm. The perforation must be strong enough for transit but weak enough to tear by hand; laminated board needs a test.
Is the ECMA X29 dieline free?
Designing on the die, the 3D fold and preflight are free in the browser. Downloading the dieline (SVG, PDF / AI, or DXF and CF2 for the die-maker) and the CMYK print PDF needs Pro.
Is Drint’s ECMA X29 exactly the FEFCO drawing?
Not exactly: Drint draws this code close to the FEFCO drawing. Check the die with your die-maker before production.